Recently, a batch of high-quality niobium plates with a thickness of 16mm passed SGS testing and was successfully produced and delivered to the customer.

The niobium plates shipped this time have a purity of over 99.95%, meet ASTM B393 standards, and will be used in the medical device field. The successful delivery of these products once again demonstrates the company's technical strength and supply capabilities in the field of deep processing of rare metal materials.

Product Features: High-Performance Refractory Metal Material

Niobium (Nb) is a rare metal with atomic number 41 and a density of 8.57 g/cm³. The 16mm niobium plates shipped this time possess the following outstanding performance characteristics:

High melting point and excellent high-temperature performance. Niobium has a melting point of up to 2468℃ (some sources report 2477℃) and a boiling point of 4742℃. It maintains excellent creep resistance even below 1650℃, making it an ideal high-temperature structural material.

Excellent corrosion resistance. Niobium exhibits excellent chemical stability to acids, alkalis, and oxidizing media. At high temperatures, a dense oxide protective layer forms on its surface, demonstrating excellent oxidation resistance.

Good processability and ductility. High-purity niobium metal possesses excellent ductility, facilitating processing into various forms such as plates, foils, and wires to meet diverse customer customization needs.

Unique superconducting properties. Niobium exhibits excellent superconductivity at low temperatures, making it a crucial foundational material in the field of low-temperature superconductivity.

ASTMB393 R04210 Niobium plate price

Medical applications: A preferred biocompatible material.

Due to its excellent biocompatibility and corrosion resistance, niobium is finding increasingly widespread applications in the medical field. The 16mm niobium plates delivered this time will primarily be used in the manufacturing of medical devices.

In the field of orthopedic implants, niobium-based materials have demonstrated significant advantages. Studies have shown that niobium possesses good biocompatibility and bioactivity. Titanium-niobium alloys exhibit high biomechanical strength and a low elastic modulus, more closely resembling human cortical bone, and have been widely used in dental, orthopedic, and artificial hip joint implant materials. Zirconium-niobium alloys are hailed in the industry as a "perfect combination of metal and ceramic," possessing both the ductility and toughness of metals and the wear resistance and biocompatibility of ceramics.

In the cardiovascular implant field, niobium-titanium alloy cardiovascular stents exhibit a corrosion rate of less than 0.01 mm/year in simulated body fluids, 80% lower than 316L stainless steel, significantly extending implant lifespan. Furthermore, niobium can be used to manufacture biocompatible components such as artificial joint connectors and pacemaker shells.

In the field of oral medicine, niobium, as a material with high biocompatibility and physicochemical properties, is used in implantology, prosthodontics, orthodontics, and maxillofacial surgery due to its relatively low elastic modulus and strong corrosion resistance. Niobium-based materials are receiving increasing attention in clinical applications in dentistry and orthopedics.

In the field of medical imaging, high-purity niobium is a primary raw material for low-temperature superconductivity and can be used in medical magnetic resonance imaging (MRI) equipment. Niobium-titanium alloy (Nb-47Ti) achieves a critical current density of 10⁵ A/cm² at 4.2 K and is widely used in MRI magnets.

ASTMB393 R04210 Niobium plate suppliers

Our company's products encompass various forms including plates, bars, tubes, wires, and foils, widely used in aerospace, medical implants, chemical corrosion protection, superconducting technology, and the electronics industry. We strictly adhere to national standards and international standards such as ASTM in our production processes and can customize niobium plates and other rare metal products to meet specific customer needs.

We will continue to uphold the business philosophy of "quality first, customer foremost," continuously improving product quality and service levels, and are committed to providing high-quality rare metal material solutions for high-end manufacturing sectors such as medical, aerospace, and chemical industries.

Tel: +86-0917- 3664600

WhatsApp: +8618791798690

sales@tmsalloy.com
tina@tmsalloy.com

Küsi pakkumist